Aluminium-base alloys which tend to form stress cracks during continuous casting are prevented from forming such cracks by incorporation in the alloys of 0.01-0.03 per cent Ti with or without 0.0025-0.01 per cent B. In an example 0.03 per cent Ti and 0.01 per cent B are added to an alloy containing 1.7 per cent Cu, 2.8 per cent Mg. 5.7 per cent Zn, 0.2 per cent Cr and the remainder Al.
机译:通过在含有或不含0.0025-0.01%B的0.01-0.03%Ti合金中掺入可防止在连续铸造过程中容易形成应力裂纹的铝基合金形成这种裂纹。在一个示例中,含有0.03%的Ti和0.01%的Ti将百分之一的B添加到含有1.7%的铜,2.8%的Mg的合金中。锌为5.7%,铬为0.2%,其余为铝。

著录项

  • 公开/公告号GB785336A

    专利类型

  • 公开/公告日1957-10-23

    原文格式PDF

  • 申请/专利权人 VEREINIGTE ALUMINIUM-WERKE AKTIENGESELLSCHAFT;

    申请/专利号GB19550015443

  • 发明设计人

    申请日1955-05-27

  • 分类号C22C21/00;

  • 国家 GB

  • 入库时间 2022-08-23 22:09:42

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号