A paint for use in air-cooled selenium rectifiers comprises an epoxy resin of molecular weight at least 1000, a pigment and a solvent, preferably in the ratio 1:2.5:5 respectively. In an example "Epikote 1009" (Registered Trade Mark) (molecular weight 3800), TiO2 and methylcyclohexanone are mixed in a weight ratio of 20:50:92.5. Aluminium silicate is also a suitable pigment.
机译:用于空气冷却的硒整流器的涂料包括分子量至少为1000的环氧树脂,颜料和溶剂,优选分别为1:2.5:5的比例。在一个实例“ Epikote 1009”(注册商标)(分子量3800)中,TiO 2和甲基环己酮以20:50:92.5的重量比混合。硅酸铝也是合适的颜料。