Procedure for the production of ferroelectric ceramic materials, of the type consisting of a ternary solid solution having the general formula Pb (Mg1/3Nb2/3) xTiyZrzO3, X, Y and Z representing the molar ratios of the components, characterized by comprising the steps de: intimately mix with distilled water the starting materials including PbO or Pb3O4 or MgCO3, Nb205 or Nb (OH) 5-, TiO2 and ZrO2, preferably together with at least one additive chosen from the group including MnO2, CoO, NiO, Fe2O3 and Cr2O3; dry the mixture; mold it under high pressure into specific shapes; calcining these forms and pulverizing them wet; drying the powder thus obtained; mold it under high pressure and in the desired shapes; polish and coat two opposing surface areas of these shapes with silver paint; cook them to form electrodes therein and finally polarize them by means of a direct voltage applied to said electrodes. (Machine-translation by Google Translate, not legally binding)
机译:生产铁电陶瓷材料的方法,该方法由具有通式Pb(Mg1 / 3Nb2 / 3)xTiyZrzO3,X,Y和Z的三元固溶体组成,代表组分的摩尔比,其特征在于包括以下步骤de:与蒸馏水充分混合包括PbO或Pb3O4或MgCO3,Nb205或Nb(OH)5-,TiO2和ZrO2的原料,优选与至少一种选自MnO2,CoO,NiO,Fe2O3和Cr2O3;干燥混合物;在高压下将其成型为特定形状;煅烧这些形式并弄湿它们;干燥由此获得的粉末;在高压下将其成型为所需的形状;用银漆打磨并涂覆这些形状的两个相对表面区域;蒸煮它们以在其中形成电极,最后通过施加到所述电极的直流电压使它们极化。 (通过Google翻译进行机器翻译,没有法律约束力)

著录项

  • 公开/公告号ES351572A3

    专利类型

  • 公开/公告日1969-06-01

    原文格式PDF

  • 申请/专利权人 MATSUSHITA ELECTRIC INDUSTRIAL CO. LIMITED;

    申请/专利号ES19680351572

  • 发明设计人

    申请日1968-03-01

  • 分类号H01F;

  • 国家 ES

  • 入库时间 2022-08-23 12:39:34

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号