首页> 外国专利> Procedure of electric welding of protective on a metal piece and device for the put into practice of this procedure. (Machine-translation by Google Translate, not legally binding)

Procedure of electric welding of protective on a metal piece and device for the put into practice of this procedure. (Machine-translation by Google Translate, not legally binding)

机译:将保护层电焊接到金属件上的程序以及该程序的实施装置。 (通过Google翻译进行机器翻译,没有法律约束力)

摘要

Method of electrical welding of protuberances on the wall of a metal part, such as a tube in which the protrusion and the tube or the like are connected to a current source, in such a way that the fact of disposing said protuberance, protected by a anti-oxidant agent, in contact with said birth tube to an arc that gives off the heat necessary for welding, said method being characterized in that it consists of limiting the application pressure of the protuberance, and therefore its penetration, to a determined value in order to prevent the deformation of the tube and the foundation of residual stresses in the metal of the tube in the course of the welding operation, because this pressure is limited by cutting off the supply current when said protrusion has traveled a certain stroke, because a local reheating of the tube or similar is carried out in the vicinity of the welding in order to avoid contraction b rusca of the metal due to the adjacent welds because, the protuberances are protected against oxidation by means of a coating paste arranged so as to form, at the end of the protrusion intended to be welded with the tube, a protective crown that overlaps axially said end, because the coating of the protuberance can be performed by immersion, compression or vibration, because after the coating of the protuberances, it is first proceeded to drying in a cold air stream for eight to twelve hours, then to a treatment in stove at a temperature of 90 to 110º for one to three hours, and because the drying time is preferably chosen for about ten hours and the oven treatment is preferably carried out for two hours at 110º. (Machine-translation by Google Translate, not legally binding)
机译:在诸如管的金属部件的壁上电连接突起的方法,其中突起和管或类似物连接到电流源上,使得布置所述突起的事实受到保护。抗氧化剂,与所述分娩管接触形成电弧,该电弧释放出焊接所需的热量,所述方法的特征在于,该方法包括将突起的施加压力及其渗透限制在一定的范围内。为了防止在焊接操作过程中管子变形和在管子金属中残留应力的产生,因为当所述突起经过一定行程时,通过切断电源电流来限制该压力,因为为了避免金属由于相邻的焊缝收缩而在焊接附近对管子或类似物进行局部再加热,以防止金属收缩。通过布置成在要与管子焊接的突出部的端部上形成涂层的涂层膏抗氧化,这是因为可以通过浸入来进行突起的涂层,压缩或振动,因为在包覆突起后,首先要在冷气流中干燥八至十二小时,然后在90至110º的温度的炉子中进行一至三小时的处理,并且干燥时间优选选择约十小时,而烤箱处理优选在110º下进行两小时。 (通过Google翻译进行机器翻译,没有法律约束力)

著录项

  • 公开/公告号ES356374A3

    专利类型

  • 公开/公告日1970-01-01

    原文格式PDF

  • 申请/专利权人 SOCIETE DES FABRICATIONS BIRAGHI - ENTREPOSE;

    申请/专利号ES19680356374

  • 发明设计人

    申请日1968-07-22

  • 分类号B23K;

  • 国家 ES

  • 入库时间 2022-08-23 11:27:39