1,214,779. Cement compositions. PORTLAND CEMENT ASSOCIATION. 4 June, 1969 [11 June, 1968], No. 28370/69. Heading ClH. A rapid set cement composition contains 1- 30% of 11CaO.7Al 2 O 3 .CaX 2 , X being halogen. 1-12% of CaSO 4 can also be present. The halo compound can be added directly to the cement or it can be formed in situ by heating cement ingredients containing an excess of A1 2 0 3 with, e.g. CaF 2 or CaCI 2 the temperature for the fluoride being 1275-1400‹ C. and for the chloride being 1380-1510‹ C. The product can be used as is, or blended with ordinary cement. Lightweight aggregates, e.g. pumice, expanded perlite or verniculite or normal ones, e.g. sand or gravel can be bonded with the cement.
机译:1,214,779。水泥组合物。波特兰水泥协会。 1969年6月4日[1968年6月11日],第28370/69号。标题ClH。快速固化的水泥组合物包含1-30%的11CaO.7Al 2 O 3 .CaX 2,X是卤素。也可以存在1-12%的CaSO 4。卤化物可以直接加入到水泥中,也可以通过例如用过量的Al 2 0 3加热水泥成分而原位形成。 CaF 2或CaCl 2,氟化物的温度为1275-1400°C,氯化物的温度为1380-1510°C。该产品可以原样使用,或与普通水泥共混。轻质骨料,例如浮石,膨胀珍珠岩或白云母或普通的,例如沙子或砾石可以与水泥粘结。

著录项

  • 公开/公告号MY7200061A

    专利类型

  • 公开/公告日1972-12-31

    原文格式PDF

  • 申请/专利权人 PORTLAND CEMENT ASSOCIATION;

    申请/专利号MY19720000061

  • 发明设计人

    申请日1972-12-30

  • 分类号C04B7/42;C04B22/00;

  • 国家 MY

  • 入库时间 2022-08-23 07:35:46

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号