首页> 外国专利> Solid electrolyte contg alumina, titania and zirconia - used in metallurgy for determining degree of oxidn. of liq. metals e.g. steel

Solid electrolyte contg alumina, titania and zirconia - used in metallurgy for determining degree of oxidn. of liq. metals e.g. steel

机译:固体电解质,包括氧化铝,二氧化钛和氧化锆-在冶金中用于确定氧化程度。的液量金属例如钢

摘要

Solid electrolyte contg., by wt., 85-95 % Al2O3, 1-5% TiO2 and 4-10% ZrO2, has raised working life, e.g. to 2-4 hrs. in uninterrupted contact with metal and 80-90% reliability in working. Props. include : 0-1 open porosity, 3.7-4.1 g/cc apparent density, 8-15 temp. change cycle stability at 1300-20 degrees C in air, 93-98% ion conductivity.
机译:固体电解质按重量计包含85-95%的Al2O3、1-5%的TiO2和4-10%的ZrO2,从而提高了使用寿命,例如到2-4小时与金属的不间断接触,工作可靠性> 80-90%。道具。包括:0-1开孔率,3.7-4.1 g / cc表观密度,8-15温度。改变空气在1300-20摄氏度下的循环稳定性,离子电导率为93-98%。

著录项

  • 公开/公告号FR2207759A1

    专利类型

  • 公开/公告日1974-06-21

    原文格式PDF

  • 申请/专利权人 VOSTOCHNY NAUCHNO ISSLESU;

    申请/专利号FR19720042265

  • 发明设计人

    申请日1972-11-28

  • 分类号B01K3/00;G01N27/00;

  • 国家 FR

  • 入库时间 2022-08-23 05:13:05

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号