The leaching soln is obtd from a hydrometallurgical process, where the soln. contains two or more ionic constituents which can be sepd. by pptn. The novelty is that the major part, but not all, of one or more constituents is pptd. in a first stage (a) and removed from the soln., and then the residual part of the constituent(s) is pptd. in a second stage(b). The amt. of constituent(s) removed in stage(a) is pref. 60-95%, and the process is pref. employed for the pptn. of Fe3+, Al and /or Cr ions from a soln. contg. Ni, Cu and/or Co. The process may also be used for the pptn. of Ni from a soln. which also contains Mg; or the pptn. of Cu from a soln. contg. Cu and Ni. The treatment is used in large scale metal winning processes where only a min. amt. of reagents is required so operating costs are reduced and environmental pollution minimised.
机译:浸出液是从湿法冶金工艺中提炼出来的。包含两个或多个可以分离的离子成分。由pptn。新颖之处在于,一种或多种成分的主要部分而不是全部都是pptd。在第一阶段(a)中将其从溶液中除去,然后将成分的剩余部分pptd。在第二阶段(b)。 AMT。在阶段(a)中删除的成分中的一个是首选。 60-95%,过程是优选的。用于pptn。溶液中的Fe3 +,Al和/或Cr离子续Ni,Cu和/或Co。该方法也可以用于pptn。锡中的镍还含有镁;或pptn。锡中的铜续铜和镍。该处理用于仅需一分钟的大规模金属制胜过程。 amt。需要使用大量试剂,因此可以降低运营成本并最大程度地减少环境污染。

著录项

  • 公开/公告号BR7602130A

    专利类型

  • 公开/公告日1976-10-05

    原文格式PDF

  • 申请/专利权人 INT NICKEL CO OF CA LTD;

    申请/专利号BR19767602130

  • 发明设计人 GARRITSEN P;BLANCO J;

    申请日1976-04-08

  • 分类号C22B3/00;

  • 国家 BR

  • 入库时间 2022-08-23 02:56:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号