Curl shrunk silk yarn prodn. - by reverse-twisting and heating under pressure sericin-free silk with absorbed collagen

机译:卷曲缩丝纱产品。 -通过逆捻并在加压下加热无丝胶的蚕丝,并吸收胶原蛋白

摘要

Sericin is removed from raw silk before absorbing collagen derived protein into it, and then twisting the yarn and saturating it with water. Next step is keeping it for 10 to 20 minutes at 130-140 degrees C under press. of 3-3.5 atmos. The yarn is then reverse-twisted and treated in saturated water vapour, so that its fibres acquired uniform curl shrinkage. Lower temp. and press. conditions than usual improve strength and durability.
机译:从生丝中除去丝胶,然后再将胶原蛋白吸收进去,然后将纱线加捻并用水浸透。下一步是将其在130-140摄氏度的压力下保持10至20分钟。 3-3.5大气压。然后将纱线反向加捻并在饱和水蒸气中进行处理,以使其纤维获得均匀的卷曲收缩率。较低温度然后按。比平常的条件提高强度和耐久性。

著录项

  • 公开/公告号DE2740046A1

    专利类型

  • 公开/公告日1979-03-08

    原文格式PDF

  • 申请/专利权人 MIZUSHIMASHIGESABURO;KOSUGIHIROSHI;

    申请/专利号DE19772740046

  • 发明设计人 BEANTRAGT NICHTNENNUNG;

    申请日1977-09-06

  • 分类号D02G1/20;

  • 国家 DE

  • 入库时间 2022-08-22 19:49:01