The amt. of O2 is measured via the electromotive force of a cell which uses a carrier (1) functioning as a reference electrode and also a conductor. Carrier (1) is coated with a layer (2) which includes gamma-Al2O3; and only after immersion in the molten metal is the gamma-Al2O3 converted into beta-Al2O3 which conducts oxygen ions so layer (2) forms the solid electrolyte. Layer (2) pref. also contains Na2O, FeO, and/or K2O; plus a flux, esp. an alkali(ne earth) fluoride, e.g. CaF2, NaF, and/or clay or felspar; and also SiO2. Carrier (1) is pref. a metal bar; and plasma flame spraying is pref. used to apply layer (2) to bar (1), followed by using compressed air at min. 5 atmos. to compact layer (2) on bar (1). Reliable determn. of active O2 even below 0.001% at temps. above 1250 degrees C, e.g. in molten cast iron.
机译:AMT。 O 2的值是通过电池的电动势来测量的,该电池使用的是用作参考电极的载体(1)以及导体。载体(1)涂覆有包括γ-Al2 O 3的层(2);并且只有在浸入熔融金属中后,γ-Al2O3才转变成β-Al2O3,它传导氧离子,因此层(2)形成了固体电解质。第(2)层偏好设定。还包含Na2O,FeO和/或K2O;加上助焊剂,特别是碱金属(氟化物)氟化物,例如CaF2,NaF和/或粘土或长石;还有SiO2载体(1)是首选。金属棒;等离子火焰喷涂是首选。用于将层(2)施加到钢筋(1)上,然后在至少2分钟使用压缩空气。 5个大气压。压实杆(1)上的层(2)。可靠的确定。临时氧气含量甚至低于0.001%。高于1250摄氏度,例如在熔融铸铁中。

著录项

  • 公开/公告号DE2916407A1

    专利类型

  • 公开/公告日1979-11-08

    原文格式PDF

  • 申请/专利权人 VEREIN FUER PRAKTISCHE GIESSEREIFORSCHUNG;

    申请/专利号DE19792916407

  • 发明设计人 MEYERWILFRIEDDR.;

    申请日1979-04-23

  • 分类号G01N27/50;

  • 国家 DE

  • 入库时间 2022-08-22 19:42:06

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号