PCT No. PCT/FR80/00151 Sec. 371 Date Jun. 16, 1981 Sec. 102(e) Date Jun. 16, 1981 PCT Filed Oct. 16, 1980 PCT Pub. No. WO81/01100 PCT Pub. Date Apr. 30, 1981.Process for hard coating with sorbitol. On the one hand, a sorbitol syrup having a concentration of 60 to 85% by weight is supplied on a moving bed of cores to be coated and, on the other hand, the temperature prevailing in the bed is kept at a value comprised between 50 DEG and 10 DEG C. The present coating process applies conveniently to cores of the "without sugar" type in the field of confectionery and pharmaceutical products.