PROCESS FOR THE SEPARATION OF COBALT FROM THE SOLUTION OF A NICKEL(II) SALT

机译:从镍(II)盐溶液中分离钴的方法

摘要

1316767 Basic Ni carbonates; removing Co from Ni solutions LE NICKEL 22 July 1970 [12 Aug 1969] 35412/70 Heading ClA A mixture of basic NiSPII/SP and NiSPIII/SP carbonates is produced by reacting a NiSPII/SP salt solution with an aqueous solution containing an alkali metal carbonate and an oxidizing alkali metal salt. The products have the formulµ respectively. The Ni salt may be sulphate, chloride or nitrate, and the oxidizing solution may contain Na 2 CO 3 and a persulphate, hypochlorite or hypobromite, preferably NaOCl. The reaction temperature may be 10-25‹ C. The product is used to remove CoSPII/SP as CoSPII/SP carbonate from NiSPII/SP solutions, e.g. sulphate, chloride, or nitrate, at 60-95‹ C. Excess Ni carbonate is used and the resulting ppt. used to treat further impure solution together with some fresh Ni carbonate; the resulting partially decobalted solution is then treated with excess fresh Ni carbonate and the cycle repeated.
机译:1316767碱式碳酸镍;从Ni溶液中去除Co镍,1970年7月22日[1969年8月12日] 35412/70标题为ClA通过使Ni反应生成碱性Ni II 和Ni III 的混合物含有碱金属碳酸盐和氧化性碱金属盐的水溶液的 II 盐溶液。产品分别具有配方。 Ni盐可以是硫酸盐,氯化物或硝酸盐,并且氧化溶液可以包含Na 2 CO 3和过硫酸盐,次氯酸盐或次溴酸盐,优选NaOCl。反应温度可以为10-25℃。该产物用于从Ni II 溶液中除去作为碳酸Co II 的Co II 。硫酸盐,氯化物或硝酸盐在60-95°C下使用。使用了过量的碳酸镍和所得的ppt。用于与一些新鲜的碳酸镍一起处理其他不纯溶液;然后将所得的部分脱钴的溶液用过量的新鲜碳酸镍处理,并重复该循环。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号