Pure CrO2 is mfd. by oxidising hydrated chromic oxide Cr2O3.xH2O, (where x is not 1). Oxidn. occurs at min. 350 degree C and min. 2 kilobars, using an oxidant which is solid or in aq. soln. The oxidant is HXOy.zH2O (where X is Cl or I; y = 1-4 and z is the water of crystallisation in the solid or the dilution of the liq.). The Cr2O3 is pref. made by adding NH3 to a soln. of CrCl3 and washing to remove NH4Cl4, then drying. The oxidants are pref. HClO4.zH2O, HIO3 or HIO4.2H2O, used at 400-500 degrees C and 2.5-4 kilobars. Prod. is used for industrial synthesis of ferromagnetic CrO2, esp. black acicular microcrystals with a rutile structure and min. Curie temp. is 120 degrees C.
机译:纯CrO2为MFD。通过氧化水合氧化铬Cr2O3.xH2O(其中x不为1)。氧化。至少在发生350摄氏度及以上2千巴,使用固体或水溶液中的氧化剂。 soln。氧化剂为HXOy.zH2O(其中X为Cl或I; y = 1-4,z为固体中的结晶水或液体的稀释液)。 Cr2O3是优选的。通过将NH3添加到溶液中制得。用CrCl 3洗涤并除去NH 4 Cl 4,然后干燥。氧化剂是优选的。 HClO4.zH2O,HIO3或HIO4.2H2O,在400-500摄氏度和2.5-4千巴下使用。产品用于工业合成铁磁性CrO2,尤其是。黑色针状微晶,具有金红石结构,最小。居里温度是120摄氏度。

著录项

  • 公开/公告号FR2327198B1

    专利类型

  • 公开/公告日1981-02-20

    原文格式PDF

  • 申请/专利权人 ANVAR;

    申请/专利号FR19750031056

  • 发明设计人

    申请日1975-10-10

  • 分类号C01G37/02;G11B5/62;

  • 国家 FR

  • 入库时间 2022-08-22 15:07:28

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号