首页> 外国专利> PROCESS FOR PRODUCING SYNTHETIC COKING COAL OF HIGH VOLATILE MATTER CONTENT

PROCESS FOR PRODUCING SYNTHETIC COKING COAL OF HIGH VOLATILE MATTER CONTENT

机译:高挥发分含量的合成焦煤生产工艺

摘要

N-4-2211GC/79ABSTRACT OF THE DISCLOSUREA process for producing a synthetic coking coal of highvolatile matter content by thermal cracking of a heavy hydro-carbon through the delayed coking process comprising heating saidheavy hydrocarbon in a furnace to a temperature between about380°C and 500°C and sufficient to initiate cracking; introducingsaid heated heavy hydrocarbon into a coking drum where it ismaintained at a temperature and for a time sufficient to effectcracking to thereby produce a thermally cracked residue havinga volatile matter content of from about 25 to 45 wt% and aGieseler fluidity of at least about 50,000 ddpm; withdrawingsaid thermally cracked residue from the coking drum at atemperature selected so as to satisfy the relation:T ? 0.293x2 - 26.12x + 790,wherein T is the temperature (°C) of the thermally crackedresidue; x is the volatile matter content of the residue (wt%)and is in the range of from about 25 to 45 wt%, and bringingsaid residue into contact with water for cooling and solidi-fication; and the synthetic coking eoal product.
机译:N-4-2211GC / 79披露摘要生产高合成焦煤的方法重型水力热裂解产生的挥发性物质含量碳通过延迟焦化过程包括加热重碳氢化合物在炉中达到约380°C和500°C,足以引发裂纹;引进所说的重碳氢化合物进入炼焦鼓保持在一定温度下并保持足够的时间裂化从而产生具有挥发性物质含量约为25至45 wt%,Gieseler的流动性至少约为50,000 ddpm;退出焦化鼓中的热裂解残留物在选择满足以下关系的温度:? 0.293x2-26.12x + 790,其中T是热裂解的温度(°C)残留物x是残留物的挥发物含量(wt%)含量约为25至45 wt%,所述残留物与水接触以冷却并固化-功能以及合成焦化油产品。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号