1. The mixture for the manufacture of wall products from TPP ash, including the initial fly ash and fine ground fly ash, characterized in that, with a delta strength and frost resistance of products, a decrease in the bulk mass of fuel consumption and an increase in the volume of waste of TPP utilization, it contains fine ground fly ash fraction less than 0.01 mm at the following ratio of components, weight. %: The source of fly ash. 85-90 Grind grain fraction less than 0, O1 mm10-15 2. The preparation of the charge by grinding the ashes, dosing and mixing the components, is distinguished by the fact that; in order to increase the strength and frost resistance of products, reduce fuel consumption and increase the volume of utilization of TPP waste, 1 O-15% by weight of initial fly ash and is ground by a wet method to obtain a slip with a humidity of 65-90% and a particle size of &; she 0, O1 mm, followed by mixing 7O weight. % of the obtained slurry with the original ash for 25 minutes, then the mixture is mixed with the rest of the slurry for 15-2 minutes. with QD
机译:1.一种用于由TPP灰生产壁产品的混合物,包括初始粉煤灰和细粉煤灰,其特征在于,由于产品的强度和耐冻性差,因此减少了油耗的总体质量, TPP废物利用量的增加,在以下组分,重量比下,它包含的细粉煤灰分数小于0.01 mm。 %:粉煤灰的来源。 85-90磨碎的颗粒分数小于0,O1 mm10-15 2.通过研磨灰,配料和混合组分来制备装料的特点是:为了提高产品的强度和抗冻性,减少燃料消耗并提高TPP废物的利用量,初始粉煤灰的重量为O的15%至15%,并通过湿法研磨以获得湿润的粉浆。为65-90%,粒径为&; 0,O1毫米,然后混合7O重量。 %的所得淤浆与原始灰分混合25分钟,然后将混合物与剩余的淤浆混合15-2分钟。与QD

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号