首页> 外国专利> METHOD OF RECOVERY OF RARE EARTH METALS FROM RESIDUE AFTER COAL COMBUSTION

METHOD OF RECOVERY OF RARE EARTH METALS FROM RESIDUE AFTER COAL COMBUSTION

机译:燃煤后从残渣中回收稀土金属的方法

摘要

The invention relates to a method for recovering rare metals from the combustion residues of various coals, in particular brown coals. The recovery is performed by digestion, more particularly by aqueous and/or dilute alkaline and/or dilute acidic digestion, where two or three of these steps can be combined in any desired order or they may be carried out separately. During digestion the concentration of the solution is monitored and the subsequent digestion steps are terminated at a desired concentration. The solid and liquid phase are then separated and the rare metals are isolated from the liquid phase while the solid phase, optionally after neutralization and/or washing can be utilized for example as a source of energy.
机译:本发明涉及一种从各种煤,特别是褐煤的燃烧残余物中回收稀有金属的方法。通过消化,特别是通过水和/或稀碱和/或稀酸消化来进行回收,其中这些步骤中的两个或三个可以以任何期望的顺序组合或者它们可以分别进行。在消化过程中,监测溶液的浓度,并以所需的浓度终止后续的消化步骤。然后分离固相和液相,并从液相中分离出稀有金属,而固相,任选地在中和和/或洗涤后,例如可以用作能源。

著录项

  • 公开/公告号PL128408B1

    专利类型

  • 公开/公告日1984-01-31

    原文格式PDF

  • 申请/专利权人

    申请/专利号PL19810233810

  • 发明设计人

    申请日1981-11-13

  • 分类号C22B7/02;

  • 国家 PL

  • 入库时间 2022-08-22 09:14:38