首页> 外国专利> method of pretreatment at high temperature through an aqueous solution of alkaline minerals in the gangue clay containing at least one element to exploit.

method of pretreatment at high temperature through an aqueous solution of alkaline minerals in the gangue clay containing at least one element to exploit.

机译:高温方法是通过在煤ue石粘土中含有至少一种要开采元素的碱性矿物水溶液进行预处理。

摘要

PCT No. PCT/FR84/00110 Sec. 371 Date Nov. 28, 1984 Sec. 102(e) Date Nov. 28, 1984 PCT Filed Apr. 18, 1984 PCT Pub. No. WO84/04333 PCT Pub. Date Nov. 8, 1984.A process for pretreatment at high temperature by means of an aqueous pretreatment solution, of crushed ores containing at least one usable metal element, whose gangue contains argillaceous compounds which, in the attack operation for making use of the ore, are capable of forming a stable plastic suspension in the presence of water, which makes it virtually impossible subsequently to separate the liquid and solid phases by virtue of its character being such that it cannot be subjected to filtration and/or settlement, which is characterized in that, to cause stabilization of the argillaceous gangue before the operation of subjecting the ore to attack and to produce easy separation of the liquid and solid phases after the attack operation, the ore, the granulometry of which is at most equal to the liberation sieve mesh size of the metal or metals to be put to use, and before being subjected to the attack operation for making use of the ore, is brought into contact with an aqueous pretreatment solution containing at least 2.10-5 g/l of OH- ions, then the medium formed is immediately raised to the minimum pretreatment temperature of at least 120 DEG C. in a period of time of at most 30 minutes reckoned from the time at which the ore is brought into contact with the aqueous pretreatment solution.
机译:PCT号PCT / FR84 / 00110第二部分371日期1984年11月28日102(e)1984年11月28日PCT日期1984年4月18日提交PCT Pub。 WO84 / 04333 PCT公开号日期为1984年11月8日,一种通过水性预处理溶液对含有至少一种可用金属元素的压碎矿石进行高温预处理的方法,该金属矿石的脉石中含有泥质化合物,在侵蚀操作中利用该矿石能够在水存在下形成稳定的塑料悬浮液,由于其特性使其无法进行过滤和/或沉降,因此几乎不可能随后分离液相和固相。在于,在使矿石受到侵蚀的操作之前使泥煤脉石稳定,并且在侵蚀操作之后使液相和固相易于分离,该矿石的粒度最大等于释放筛。将要使用的一种或多种金属的网眼尺寸与进行矿石利用的浸蚀操作之前接触在含有至少2.10-5 g / l OH-离子的预处理水溶液中,然后将形成的介质在最多30分钟的时间内立即升高到至少120℃的最低预处理温度,从使矿石与预处理水溶液接触的时间。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号