Process comprises addn. to the fresh concrete of 0.5-1 percent relative to the cement weight, of an aqueous solution contg. 1-4 parts/thousand polyvinyl pyrrolidone as non-inorganic protective colloid, and 0.8-1.2 of phosphoric acid butyl ester. After hardening in a mould, the temperature of the concrete is lowered several deg.C relative to room temp. over one hour. - The addn. is made to the powder form concrete mix, in conjunction with plasticising, sealing, pore-forming, accelerating and retarding agents. (0/0)
机译:过程包括addn。相对于水泥重量为0.5-1%的新混凝土的水溶液(续)。 1-4份/千个聚乙烯吡咯烷酮作为非无机保护胶体,以及0.8-1.2份磷酸丁酯。在模具中硬化后,混凝土的温度相对于室温降低了几摄氏度。一小时以上。 -addn。是将粉末状混凝土混合物与增塑剂,密封剂,成孔剂,促进剂和缓凝剂一起制成的。 (0/0)

著录项

  • 公开/公告号ES517416A0

    专利类型

  • 公开/公告日1983-12-16

    原文格式PDF

  • 申请/专利权人 LUDWIG HOERLING FABRIK CHEM BAUSTOFFE GMBH;

    申请/专利号ES19820517416

  • 发明设计人

    申请日1982-11-16

  • 分类号C04B31/30;

  • 国家 ES

  • 入库时间 2022-08-22 09:07:10

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号