A process for producing a binder (cement) to be used in slurry, mortar, or concrete having a low water-to-cement ratio. As raw-material for the binder is used at least 50% by weight of a hydraulic material, such as slag, technical pozzolanas and/or natural pozzolanas. The hydraulic material is ground to a specific surface of at least 400 m2/kg. To the raw-material is added 0.1 to 5% by weight of a plasticizing material, such as a sulphonated polyelectrolyte. To the raw-material are also added in total 0.5 to 8% by weight of sodium carbonate and/or sodium hydroxide. Added in small amounts, the sodium carbonate and the sodium hydroxide, separately or in combination, considerably shorten the hardening time of the concrete, yield excellent strengths, and make it possible to use cheap raw-materials.
机译:一种用于水灰比低的泥浆,砂浆或混凝土中的粘结剂(水泥)的生产方法。作为粘合剂的原料,使用至少50重量%的水硬性材料,例如矿渣,工业火山灰和/或天然火山灰。将液压材料研磨至至少400 m2 / kg的比表面。向原料中添加0.1至5重量%的增塑材料,例如磺化聚电解质。也向原料中总共添加0.5至8重量%的碳酸钠和/或氢氧化钠。少量或单独添加碳酸钠和氢氧化钠,可大大缩短混凝土的硬化时间,产生优异的强度,并可以使用廉价的原材料。

著录项

  • 公开/公告号CH644573A5

    专利类型

  • 公开/公告日1984-08-15

    原文格式PDF

  • 申请/专利权人 FLOWCON OY;

    申请/专利号CH19800004241

  • 发明设计人 BENGT FORSS;

    申请日1980-05-30

  • 分类号C04B31/02;C04B13/00;C04B15/00;

  • 国家 CH

  • 入库时间 2022-08-22 08:51:32

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号