A low carbon, vacuum degassed steel containing columbium, titanium and/or zirconium, having high ductility, no yield point elongation in the hot rolled and cold rolled and annealed conditions. The steel contains from 0.002 to 0.020 percent carbon, up to 0.60 percent manganese, from greater than 0.025 to 0.12 percent columbium, titanium when present from 0.015 to 0.12 percent, zirconium when present from 0.028 to 0.18 percent, up to 0.008 percent nitrogen, up to 0.010 percent total oxygen, up to 0.035 percent sulfur, up to 0.045 percent total aluminum, and balance substantially iron. The steel has extra-deep drawing quality.
机译:一种低碳,真空脱气的钢,含co,钛和/或锆,具有高延展性,在热轧和冷轧及退火条件下无屈服点伸长。该钢含有0.002-0.020%的碳,高达0.60%的锰,大于0.025-0.12%的,、钛(含量为0.015%至0.12%),锆(含量为0.028-0.18%),氮含量高达0.008%总氧含量为0.010%,硫含量最高为0.035%,铝含量最高为0.045%,铁基本平衡。这种钢具有超深的拉拔质量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号