首页> 外国专利> SHORT-TIME HEAT TREATMENT OF SAME-METAL WELDED PART OF LOW-TEMPERATURE STEEL PIPE CONTAINING NI

SHORT-TIME HEAT TREATMENT OF SAME-METAL WELDED PART OF LOW-TEMPERATURE STEEL PIPE CONTAINING NI

机译:含镍低温钢焊接件的短时热处理

摘要

PURPOSE:To improve remarkably the low-temp. toughness of the same-metal welded part by heat-treating the same-metal welded part under specified conditions when a low-temp. steel pipe contg. Ni is welded by using a same-metal welding material and then the same-metal welded part is hardened and tempered. CONSTITUTION:When a low-temp. steel pipe contg. Ni is welded by using a same-metal welding material and then the same-metal welded part is submitted to short-time hardening and tempering, the same-metal welded part is kept at 550-650 deg.C for 1-10min before the part is hardened to improve the low-temp. toughness of the same-metal welded part. The welding material is preferably composed of =about 0.08% C, about 0.01-0.45% Si, about 0.3-1.0% Mn, =about 0.01% P, =about 0.01% S, =about 0.035% O, =about 0.01% N, and the remainder of an appropriate amt. of Ni, Fe, and inevitable impurities.
机译:目的:显着改善低温。低温条件下,在规定条件下对同一金属焊接零件进行热处理,从而获得该金属焊接零件的韧性。钢管续通过使用相同金属的焊接材料焊接Ni,然后对相同金属的焊接部件进行淬火和回火。组成:低温时。钢管续使用相同金属的焊接材料对镍进行焊接,然后对相同金属的焊接零件进行短时的淬火和回火处理,然后将相同金属的焊接零件在550-650℃下保持1-10分钟。零件硬化以改善低温。同金属焊接零件的韧性。焊接材料优选地由≤约0.08%的C,约0.01-0.45%的Si,约0.3-1.0%的Mn,≤约0.01%的P,≤约0.01%的S,≤约0.035%的O,≤ =约0.01%N,其余为适当的amt。 Ni,Fe和不可避免的杂质。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有