1. Method for preparing a porous ceramic or glass-ceramic or glassy coating on an article, on the one hand, or a porous ceramic or glass-ceramic or glassy self-supporting body, on the other hand, including the following steps : (a) a ceramic or glass-ceramic or glassy mass is made and ground to a powder, (b) the powder is mixed with water, (c) the mixture is either applied in a layer to the article to be provided with the coating or is formed into the body, (d) the layer or the body according to (c) is pre-dried, (e) the pre-dried layer or the pre-dried body according to (d) is fired and, if required, is then subjected to a controlled heat treatment for adjusting the crystal fraction formed in the coating or in the self-supporting body, characterized by the following step between steps (b) and (c) : (b1) the mixture according to (b) is maintained at a temperature from 40 degrees to 200 degrees C for a time period which enables water to bind chemically with the powder.
机译:1.一方面在制品上制备多孔陶瓷或玻璃陶瓷或玻璃状涂层的方法,另一方面,在多孔陶瓷或玻璃陶瓷或玻璃状自支撑体上的制备方法,包括以下步骤: a)制成陶瓷或玻璃陶瓷或玻璃状物料并将其研磨成粉末,(b)将粉末与水混合,(c)将混合物以一层形式施加到要提供涂层的物品上,或将其成型为主体,(d)将根据(c)的层或主体预干燥,(e)将根据(d)的预干燥层或预干燥的主体烧成,如果需要,然后对其进行受控的热处理,以调节在涂层或自支撑体中形成的晶体比例,其特征在于步骤(b)和(c)之间的以下步骤:(b1)根据(b)的混合物保持在40℃至200℃的温度一段时间,使水与粉末化学结合。

著录项

  • 公开/公告号EP0121782B1

    专利类型

  • 公开/公告日1986-09-10

    原文格式PDF

  • 申请/专利权人 PFAUDLER-WERKE AG;

    申请/专利号EP19840102499

  • 发明设计人 HORSCH RUDI;

    申请日1984-03-08

  • 分类号C04B38/06;C03C11/00;C03B19/08;B24B7/24;B24C1/06;C03C15/00;

  • 国家 EP

  • 入库时间 2022-08-22 07:35:53

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号