PREPARATION METHOD OF IRON OXIDE FOR FERRITE MAGNETIC MATERIAL

机译:铁氧体磁性材料氧化铁的制备方法

摘要

PURPOSE:To form an impurity eliminated ferrite of high quality by a metod wherein crude iron oxide obtained from a residue of a zinc refining is pressed and leached through a mineral acid and then, it is mixed with iron chloride and is roasted through aeration. CONSTITUTION:A zinc leaching residue in a wet zinc refining is leached through acid and from this leached liquid, iron is precipitated in a hematitic type and crude iron oxide is separated. This crude iron oxide is leached by pressure through a mineral acid (HNO3, H2SO4, HCl) and Zn, Ca, Al2O3 and others are leached. Next thereto, iron chloride is added thereto, and the leached liquid is roasted (less than 900 deg.C) by aeration and S and As are effectively eliminated. The elimination of S and As can be performed in a low temperature, as a result, grinding after a sintering becomes easy. With this, from a residue of a zinc refining, an impurity eliminated ferrite of high quality can be formed.
机译:用途:为了形成一种高品质的去除杂质的铁素体,其中将从锌精炼残渣中获得的粗氧化铁经加压并通过无机酸浸出,然后与氯化铁混合并通过曝气焙烧。组成:湿锌精炼中的锌浸出残渣通过酸浸出,并从这种浸出的液体中以铁杂形式沉淀出铁,并分离出粗氧化铁。粗氧化铁经压力浸出后通过无机酸(HNO3,H2SO4,HCl)浸出,Zn,Ca,Al2O3等浸出。接下来,向其中添加氯化铁,并通过曝气焙烧沥滤的液体(小于900℃),并有效地消除了S和As。 S和As的消除可以在低温下进行,结果,烧结后的研磨变得容易。由此,可以从锌精炼的残渣形成高质量的杂质去除铁素体。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号