Spray-dried particles ("beads") for use as or in detergent compsns. comprise (a) 5-60 wt.% of a water-softening aluminosilicate; (b) 2-40 wt.% of bentonite contg. sufficient moisture to facilitate its dispersion so as to inhibit deposition of the aluminosilicate on linen during washing; (c) 5-60 wt.% of one or more water-soluble builders; (d) 0-30 wt.% of a water-soluble synthetic organic detergent; and (e) 0-5 wt.% of a water-soluble silicate. The particles pref. have a bulk density of 0.2-0.9 (esp. 0.2-0.8) g/cc and a particle size of 0.149-2.00 mm. Component (a) is pref. a hydrated A zeolite with an H2O content of 15-25 wt.% and a Ca exchange capacity of 200-400 meq/g. The particles are free-flowing and have a reduced tendency to deposit solids owing to the fact that they contain bentonite and little or no soluble silicate. -
机译:喷雾干燥的颗粒(“珠子”),可用作洗涤剂成分或在洗涤剂成分中使用。包含(a)5-60重量%的水软化铝硅酸盐; (b)2-40 wt。%的膨润土(续)。足够的水分以利于其分散,从而抑制洗涤过程中铝硅酸盐在亚麻布上的沉积; (c)5-60 wt。%的一种或多种水溶性助洗剂; (d)0-30重量%的水溶性合成有机洗涤剂; (e)0-5重量%的水溶性硅酸盐。颗粒优选。具有0.2-0.9(尤其是0.2-0.8)g / cc的堆积密度和0.149-2.00mm的粒度。组分(a)是优选的。 H 2 O含量为15-25重量%且Ca交换容量为200-400meq / g的水合沸石。由于颗粒含有膨润土而几乎没有或不含可溶性硅酸盐,因此颗粒是自由流动的并且具有降低的沉积固体的趋势。 --

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号