Hot-rolled steel sheet manufacturing process by hot-rolling process control

机译:通过热轧工艺控制的热轧钢板制造工艺

摘要

Carbon steel is hot-cooled, control-cooled from cooling start temperature of 800-900 deg.C to coiling temperature of 300-600 deg.C at the cooling rate of 10-100 deg.C/sec, and air-cooled. The steel comprises (in wt.%) 0.05-0.20 C, 0.1-1.5 Mn, 0.01-0.3 Si, 0.001-0.09 Sol, Al, 0.001-0.04 P, 0.001-0.04 S and balance Fe.
机译:碳钢被热冷却,以10-100℃/秒的冷却速率从800-900℃的冷却开始温度到300-600℃的卷取温度进行控制冷却,然后进行空气冷却。该钢包含(以重量%计)0.05-0.20 C,0.1-1.5 Mn,0.01-0.3 Si,0.001-0.09 Sol,Al,0.001-0.04 P,0.001-0.04 S和余量的Fe。