Poly(ethylene terephthalate) resin and blends of poly(ethylene terephthalate) resin with other polymers are extruded while being coupled with an organic diisocyanate under conditions where carbon dioxide gas is vented smoothly, as it is formed. The extruder has a number of zones designed to perform specific functions. The temperature in the kneading zone and in the venting zone must be maintained at about 280 DEG -320 DEG C. to bring about rapid reaction and to permit efficient gas evolution and removal without thermally degrading the polymeric material. The extruded article is free of trapped gas bubbles and other imperfections. This process is particularly suitable for making PET billets, which then are stretched to form strapping useful in packaging applications.
机译:聚对苯二甲酸乙二酯树脂和聚对苯二甲酸乙二酯树脂与其他聚合物的共混物在与有机二异氰酸酯偶联的同时,在二氧化碳气体顺利形成的条件下挤出,同时进行挤出。挤出机具有多个设计用于执行特定功能的区域。捏合区和通风区的温度必须保持在约280-320℃,以引起快速反应并允许有效的放出和除去气体而不会使聚合物材料热降解。挤出的制品没有气泡和其他缺陷。该方法特别适合于制造PET坯料,然后将其拉伸以形成可用于包装应用的捆扎带。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号