首页> 外国专利> IMPROVEMENT ON PROCESSABILITY OF PPE-POLYSTYRENE ANTISTATIC BLEND BY ADDITION OF STYRENE-ACRYLIC ACID COPOLYMER

IMPROVEMENT ON PROCESSABILITY OF PPE-POLYSTYRENE ANTISTATIC BLEND BY ADDITION OF STYRENE-ACRYLIC ACID COPOLYMER

机译:苯乙烯-丙烯酸共聚物的添加对PPE-苯乙烯类抗静电混合物加工性能的改进

摘要

PURPOSE: To obtain the blend having an excellent antistatic property, melt flow performance, etc. by compounding a polyphenylene ether resin, an alkenyl arom. resin copolymerized with an olefinic acid and a specific reforming additive. ;CONSTITUTION: (A) 100 pts.wt. (hereafter pts.) mixture composed of (a) 1 to 99 pts. polyphenylene ether resin [e.g. poly(2,6-dimethyl-1,4-phenylene)ether] and (b) 90 to 1 pts. another thermoplastic polymer (e.g. rubber modified impact resistant PS resin) not contg. the olefinic resin at need, (B) 1.0 to 15.0 pts. alkenyl arom. resin copolymerized with the olefinic acid (e.g. a copolymer of acrylic acid and PS resin) and (C) 1 to 15 pts. at least one kind of the reforming additive [e.g. methyl-octyl-bis(2-hydroxyethyl)ammonium paratoluene sulfonate] which is preferably an antistatic agent and is sucked to the olefinic acid of the component B are mixed.;COPYRIGHT: (C)1989,JPO
机译:用途:通过将聚苯醚树脂和链烯基芳烃混合,可获得具有优异的抗静电性能,熔体流动性能等的共混物。与烯酸和特定的重整添加剂共聚的树脂。 ;组成:(A)100 pts.wt.。 (以下为点)由(a)1至99点组成的混合物。聚苯醚树脂[例如聚(2,6-二甲基-1,4-亚苯基)醚]和(b)90至1分。未接续的另一种热塑性聚合物(例如橡胶改性的抗冲击PS树脂)。 (B)1.0至15.0 pts所需的烯烃树脂。烯基芳基。与烯酸(例如丙烯酸和PS树脂的共聚物)和(C)1至15 pt共聚的树脂。至少一种重整添加剂[例如混合优选被用作抗静电剂并被吸到组分B的烯烃酸中的甲基-辛基-双(2-羟乙基)对甲苯磺酸铵盐。; COPYRIGHT:(C)1989,JPO

著录项

  • 公开/公告号JPS64156A

    专利类型

  • 公开/公告日1989-01-05

    原文格式PDF

  • 申请/专利权人 GENERAL ELECTRIC CO GE;

    申请/专利号JP19880115024

  • 发明设计人 ROBAATO JIEI AKUSERUROTSUDO;

    申请日1988-05-13

  • 分类号C08K5/17;C08L25/04;C08L67/00;C08L69/00;C08L71/00;C08L71/12;C08L77/00;

  • 国家 JP

  • 入库时间 2022-08-22 06:41:18

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号