PRODUCTION OF FLUORINE-CONTAINING SILICONE-MODIFIED NOVOLAK RESIN AND EPOXY RESIN COMPOSITION

机译:含氟硅酮改性酚醛清漆树脂和环氧树脂组合物的生产

摘要

PURPOSE:To obtain the subject resin having high glass transition point, giving a cured material having excellent crack resistance and moisture resistance and useful as a sealant for semiconductor, by reacting a novolak resin with a specific fluorine-containing organopolysiloxane and compounding the product with an epoxy resin. CONSTITUTION:The objective fluorine-containing silicone-modified novolak resin can be produced by reacting a novolak resin with a fluorine-containing organopolysiloxane of formula I [R1 is 1-8C alkyl or phenyl; R2 is H, amino, epoxy, hydroxy, halogen or alkoxy; Rf is group of formula II (n is integer of 1-5), formula III, formula IV (m is integer of 3-10), formula V, formula VI (l is integer of 2-6) or formula VII (R is H or methyl); X=0; Y=1 and Z is integer or =1]. An epoxy resin composition having excellent crack resistance is obtained by compounding the above resin with an epoxy resin and a hardener.
机译:用途:通过使线型酚醛清漆树脂与特定的含氟有机基聚硅氧烷反应,然后将产物与苯甲酸酯混合,可得到具有高玻璃化转变温度的主题树脂,从而获得具有优异的耐裂性和耐湿性并可用作半导体密封剂的固化材料。环氧树脂。组成:目标含氟硅氧烷改性的线型酚醛清漆树脂可通过使线型酚醛清漆树脂与式I [R 1为1-8C烷基或苯基]的含氟有机聚硅氧烷反应制得; R 2为H,氨基,环氧,羟基,卤素或烷氧基; Rf是式II的基团(n是1-5的整数),式III,式IV(m是3-10的整数),式V,式VI(l是2-6的整数)或式VII的基团(R是H或甲基); X> = 0; Y> = 1,Z为整数或> = 1]。通过将上述树脂与环氧树脂和硬化剂混合,可以得到具有优异的抗裂性的环氧树脂组合物。

著录项

  • 公开/公告号JPH01315424A

    专利类型

  • 公开/公告日1989-12-20

    原文格式PDF

  • 申请/专利权人 SHIN ETSU CHEM CO LTD;

    申请/专利号JP19880147838

  • 申请日1988-06-15

  • 分类号C08G81/00;C08G59/00;C08G59/40;C08G59/62;C08L63/00;

  • 国家 JP

  • 入库时间 2022-08-22 06:23:10

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号