PURPOSE:To obtain a solid-acid catalyst hardly suffering from deactivation by having a compound of W or Mo added to or supported by zirconium oxide in a specified proportion and the making the catalyst highly acidic. CONSTITUTION:Tungsten or molybdenum compound of 1-40wt.% in terms of its metal weight is added to or supported by zirconium hydroxide or amorphous zirconium oxide. Then, it is baked at 500-1,000 deg.C and made its acidity to be stronger than pH11.9. The solid-acid catalyst thus obtained hardly suffers from deactivation in such reactions as decomposition, a isomerization and alkylation of hydrocarbons etc., and it is possible to carry out miscellaneous reactions in mild reaction conditions.
机译:用途:通过将W或Mo的化合物按指定比例添加到氧化锆或由氧化锆支撑来获得几乎不失活的固体酸催化剂,并使该催化剂呈高酸性。组成:将金属重量为1-40%(重量)的钨或钼化合物添加到氢氧化锆或无定形氧化锆中或由其负载。然后,将其在500-1,000℃下烘烤,使其酸度强于pH11.9。由此获得的固体酸催化剂在诸如分解,烃的异构化和烷基化等反应中几乎不失活,并且可以在温和的反应条件下进行各种反应。

著录项

  • 公开/公告号JPH01288339A

    专利类型

  • 公开/公告日1989-11-20

    原文格式PDF

  • 申请/专利权人 NIPPON MINING CO LTD;

    申请/专利号JP19880114790

  • 发明设计人 ARATA KAZUSHI;HINO MAKOTO;

    申请日1988-05-13

  • 分类号B01J23/28;B01J23/30;C07B61/00;C07C1/00;C07C2/62;C07C4/18;C07C5/27;C07C9/00;C07C9/16;C07C11/06;C07C15/04;C07C45/00;C07C45/46;C07C47/052;C07C49/784;C07C67/00;

  • 国家 JP

  • 入库时间 2022-08-22 06:22:42

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号