1. A process for continuously coking hard coal pitch to produce a calcinated formed coke comprised of the following process stages : - low-temperature carbonization of the approx. 300 degrees C hot hart pitch being employed to produce a low-temperature coke with a temperature of less than 600 degrees C, - briquetting of low-temperature coke with admixture of hot binder hard pitch, - calcination of briquettes at temperatures of up to approx. 1.400 degrees C, and - subsequent cooling of briquettes, characterized in that the calcination is carried out in an indirectly fired vertical chamber slot-type oven and that a rich gas is generated which after cleaning and cooling serves for indirect heating at the low-temperature carbonization stage and/or calcinating stage or for other purposes.
机译:1.连续焦化硬煤沥青以生产煅烧的成形焦炭的方法,该方法包括以下工艺步骤:-约10℃的低温碳化。使用300摄氏度的热哈氏沥青生产温度低于600摄氏度的低温焦炭-低温焦煤与热粘结剂硬沥青的混合物团块化-在最高约25摄氏度的温度下煅烧煤饼。 1.400摄氏度,以及随后的煤球冷却,其特征在于,煅烧是在间接燃烧的垂直腔狭缝式烤箱中进行的,并且产生了富气体,在清洗和冷却后,该气体用于在低温下进行间接加热碳化阶段和/或煅烧阶段或用于其他目的。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号