A process and an apparatus for the production of printed coated films in which at least one plastic-containing, prepolymer- and/or precondensate-containing, non-heat-sealable outer layer (3) having a total thickness (measured after curing or drying) of from 2 to 40 mu m and containing free reactive chemical groups and coloured pigments and/or dyes and containing at least one solvent and/or diluent of more than 35 % by weight and/or liquid monomers and/or liquid prepolymers or precondensates is applied to a plastic release film (1) at temperatures between 10 DEG C and 90 DEG C, preferably from 20 DEG C to 60 DEG C, and a 10 to 95 mu m thick, transparent or translucent coating (5) having a coloured pigment content of less than 3 % by weight and made from a coating material which can be cured by means of electron beams is applied immediately on top of the outer layer or on top of an intermediate layer arranged above the outer layer, and the coating is cured with exposure to electron beams, and the coated film formed on the release plastic film after curing is peeled off the release plastic film. IMAGE
机译:用于生产印刷涂膜的方法和设备,其中至少一个总厚度(在固化或干燥后测量)的含塑料的,含预聚物和/或预缩合物的不可热封外层(3) )为2至40μm,并且包含游离的反应性化学基团和有色颜料和/或染料,并且包含至少一种按重量计超过35%的溶剂和/或稀释剂和/或液体单体和/或液体预聚物或预缩合物在10℃至90℃,优选20℃至60℃的温度下,将其涂在塑料脱模膜(1)上,并涂有厚度为10至95μm的透明或半透明的有色涂料(5)。由可通过电子束固化的涂料制成的颜料含量小于3%(重量),应立即施加在外层顶部或布置在外层上方的中间层顶部,并且暴露于电子bea固化1ms后,将固化后的剥离塑料膜上形成的涂膜从剥离塑料膜上剥离。 <图像>

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号