首页> 外国专利> METHOD OF TESTING FLAT PLATE SPECIMENS WITH RESIDUAL WELD STRESSES FOR CORROSION CRACKING

METHOD OF TESTING FLAT PLATE SPECIMENS WITH RESIDUAL WELD STRESSES FOR CORROSION CRACKING

机译:带有残余焊接应力的平板试样腐蚀开裂的方法

摘要

the invention u043eu0442u043du043eu0441u0438u0442u0441u00a0 to u0438u0441u043fu044bu0442u0430u043du0438u00a0u043c welded connections. the purpose of u0438u0437u043eu0431u0440u0435u0442u0435u043du0438u00a0 - reducing material consumption. method u0438u0441u043fu044bu0442u0430u043du0438u00a0 samples in the form of flat plates with residual welding u043du0430u043fu0440u00a0u0436u0435u043du0438u00a0u043cu0438 corrosive cracking u0437u0430u043au043bu044eu0447u0430u0435u0442u0441u00a0 is that the u0432u044bu043fu043eu043bu043du00a0u044e t u043fu0435u0440u0435u0441u0435u043au0430u044eu0449u0438u0435u0441u00a0 welds in a direction from the periphery to the center u043bu0435u0433u0438u0440u043eu0432u0430u043du0438u00a0 welding materials of various systems.in the working area are plots of welds to the place of a limited area of the circle described on a square with side equal to the width of the stitch. the sample is maintained in corrosion environment and u043eu043fu0440u0435u0434u0435u043bu00a0u044eu0442 u0432u0440u0435u043cu00a0 to u043fu043eu00a0u0432u043bu0435u043du0438u00a0 cracks, which u0441u0443u0434u00a0u0442 sustainability model for corrosion cracking. 1 il.
机译:本发明将焊接连接件连接到 u0438 u0441 u043f u044b u044b u0442 u0430 u043d u0438 u00a0 u043c焊接连接。 u043e u0442 u043d u043e u0441 u0438 u0442 u0441 u0438 u0437 u043e u0431 u0440 u0435 u0442 u0435 u043d u0438 u00a0的目的-减少材料消耗。方法 u0438 u0441 u043f u044b u0442 u0430 u043d u0438 u00a0带有残留焊接的平板形式的样品 u043d u0430 u043f u0440 u00a0 u0436 u0435 u043d u043d u0438 u00a0 u00a0 u043c u0438腐蚀开裂 u0437 u0430 u043a u043b u044e u0447 u0430 u0435 u0442 u0441 u00a0是 u0432 u044b u043f u043e u043e u043b u043d u00a0 u044e t u0435 u0440 u0435 u0441 u0435 u043a u0430 u044e u0449 u0438 u0435 u0441 u00a0在从外围到中心的方向上进行焊接 u043b u0435 u0433 u0438 u0440 u043e u0432 各种系统中的焊接材料。在工作区域中,是在正方形的侧面(等于针迹的宽度)上描述的圆的有限区域的位置上的焊缝图。样品保持在腐蚀环境中,并且 u043e u043f u0440 u0435 u0434 u0435 u043b u00a0 u044e u0442 u0432 u0440 u0435 u043c u00a0至 u043f u043e u00a0 u0432 u043b u0435 u043d u0438 u00a0裂纹,其中 u0441 u0443 u0434 u00a0 u0442可持续性模型用于腐蚀裂纹。 1升

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号