Usage: The invention relates to ferrous metallurgy and to a method of preparing boron-containing steel of pig iron. SUMMARY proposals lies in the fact that in the melting of iron steel is used, which components are taken in the following ratio,% by weight carbon 4.0-5.0.; 0,35-1,00 silicon, manganese, 0.1-1.5; Forest 0,015-0,040; remainder iron, with the ratio of silicon to boron concentration then taken within 23-25 ​​C. with known methods of smelting borsoder--containing steels by doping boron alloy 1, boron or other boron-containing waste materials 2. vj .vi iO CJ VI 4
机译:用途:本发明涉及黑色冶金以及制备生铁的含硼钢的方法。发明内容建议在于,在铁水的熔化中使用以下成分,碳的重量百分比为4.0-5.0。 0,35-1,00硅,锰0.1-1.5;森林0,015-0,040;其余的铁,则硅与硼的浓度之比在23-25℃之内。用掺杂硼合金1,硼或其他含硼废料的方法熔炼含硼的钢的已知方法2。vj .vi iO CJ VI 4

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号