首页> 外国专利> Thermoplastic polycarbonate(s) - useful as a source of carbon di:oxide blowing agent for prodn. of thermoplastic polycarbonate foam

Thermoplastic polycarbonate(s) - useful as a source of carbon di:oxide blowing agent for prodn. of thermoplastic polycarbonate foam

机译:热塑性聚碳酸酯-可用作产品的二氧化碳发泡剂的来源。热塑性聚碳酸酯泡沫

摘要

Thermoplastic polycarbonates (I) are useful for foaming thermoplastic polycarbonates. Also claimed is a process for the prodn. of polycarbonate foam prods., by mixing (I) (with Mw = 5000-50,000) with 0.01-1 mol. % transesterification catalysts and 0.1-5 mol. % aromatic polycarboxylic acids and/or 0.1-5 mol. % water and opt. with 0.1-5 mol.% aliphatic hydroxycarboxylic acids and/or aliphatic alcohols (w.r.t. mols. of carbonate units of formula -O-R-O-CO- (with R = diphenolate residuel, and injection moulding or extruding this mixt. at 210-340 deg. C, with reaction times of 0.5-5 mins. Foam prods. (II) obtd. by this process are also claimed as such. Specifically the above process is carried out with addn. of normal additive(s); additive-contg. polycarbonate foam prods. (II) are also claimed. USE/ADVANTAGE - Foam prods. (II) are useful, eg. for the prodn.of lamp covers, housings, office equipment, parts of cabinets, etc. The invention enables the prodn. of thermoplastic polycarbonate foam by using, as blowing agent, the CO2 produced by controlled partial decompsn. of (I); the prods. (II) have a light colour, uniformly fine pore structure and smooth surfac
机译:热塑性聚碳酸酯(I)可用于使热塑性聚碳酸酯发泡。还要求保护一种产品的方法。通过将(I)(Mw = 5000-50,000)与0.01-1摩尔%的聚碳酸酯泡沫产品混合。 %的酯交换催化剂和0.1-5mol。 %的芳族多元羧酸和/或0.1-5mol。 %水和选择。用0.1-5摩尔%的脂族羟基羧酸和/或脂族醇(WRT摩尔的式-ORO-CO-的碳酸酯单元(R =二酚残基1,并在210-340℃下注塑或挤出该混合物)。反应时间为0.5-5分钟的C,也要求保护通过该方法获得的泡沫产品(II),特别是在上述方法中添加普通添加剂;与添加剂混合的聚碳酸酯用途/优点-泡沫产品(II)可用于例如灯罩,外壳,办公设备,橱柜的零件等产品。通过将(I)的受控部分分解产生的CO2用作发泡剂来制备热塑性聚碳酸酯泡沫;产品(II)具有浅色,均匀的细孔结构和光滑的表面

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号