STEEL IMPROVED IN DEEP DRAWABILITY, AND PRODUCTION OF STEEL SHEET FOR DEEP DRAWING

机译:深冲性提高的钢及深冲用钢板的生产

摘要

PURPOSE: To produce a steel improved in deep drawability by blending specified ratios of C, Mn, S and Al into iron. ;CONSTITUTION: A steel contg., by weight, ≤0.015% C, 0.15 to 0.25% Mn, ≤0.012% S, ≤0.04% Al, and the balance Fe is prepd. to obtain the steel improved in deep drawability. Moreover, this steel is produced by a converter, and the whole body is subjected to hot rolling in an austentic region, is coiled at a temp. of 650°C, preferably, at a temp. of 700°C and is continuously annealed at a temp. of ≥650°C, preferably, at a temp. of ≤700°C, thereby, the thin steel sheet suitable for a deep drawn vessel can be obtd.;COPYRIGHT: (C)1993,JPO
机译:目的:通过将指定比例的C,Mn,S和Al混入铁中来生产深冲性得到改善的钢。组成:钢,按重量计包括≤0.015%C,0.15至0.25%Mn,≤0.012%S,≤0.04%Al,其余为Fe。从而获得深拉深性得到改善的钢。另外,该钢由转炉制造,在奥氏体区域内进行整体热轧,并在一定温度下卷取。最好在温度为650℃下进行。温度为700°C,并在一定温度下连续退火。 ≥650°C,最好在温度下。 ≤700°C,因此可以制成适用于深冲容器的薄钢板。;版权所有:(C)1993,日本特许厅

著录项

  • 公开/公告号JPH05195147A

    专利类型

  • 公开/公告日1993-08-03

    原文格式PDF

  • 申请/专利权人 SOLLAC;

    申请/专利号JP19920197570

  • 申请日1992-07-01

  • 分类号C22C38/00;C21D8/04;C21D9/48;C22C38/06;

  • 国家 JP

  • 入库时间 2022-08-22 05:15:19

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号