PROCESS FOR A SELECTIVE FLOTATION OF COPPER-LEAD-ZINC SULFIDE ORES In a process for a selective flotation of a copper-lead-zinc sulfide ore the raw ore is ground and slurried with water and the resulting suspension is aerated with air to adjust a certain oxidation-reduction potential and is subsequently successively conditioned with SO2, Ca(OH)2, and collecting and frothing agents, whereafter a flotation of Cu is effected. An oxidation-reduction potential which is 70 to 90% of the oxidation-reduction potential desired for the flotation of Cu is adjusted by the aeration of the suspension with air before the flotation of Cu, the desired oxidation-reduction potential of 60 to 340 mV is adjusted during the flotation of Cu by the aeration with air, the flotation of Cu is effected at a pH of 8.5 to 10.5 and Cu is removed from the flotation process with the froth.
机译:铜铅锌硫化矿石的选择性浮选过程在铜铅锌硫化矿石的选择性浮选过程中,将原始矿石磨碎并用水打浆,然后将所得悬浮液用空气充气以调节一定的比例。氧化还原电位,随后依次用SO2,Ca(OH)2和收集和发泡剂进行调理,然后进行Cu的浮选。通过在浮选铜之前用空气对悬浮液进行曝气,可以调节浮选所需的铜的氧化还原电位的70%至90%的氧化还原电位,所需的氧化还原电位为60至340 mV在用空气充气浮选铜的过程中,调节pH值,在pH为8.5-10.5的条件下进行浮选,并用泡沫从浮选过程中除去铜。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号