In a process for a selective flotation of a copper-lead-zinc sulfide ore the raw ore is ground and slurried with water and the resulting suspension is aerated with air to adjust a certain oxidation- reduction potential and is subsequently successively conditioned with SO. sub.2, Ca(OH).sub.2, and collecting and frothing agents, whereafter a flotation of Cu is effected. An oxidation-reduction potential which is 70 to 90% of the oxidation-reduction potential desired for the flotation of Cu is adjusted by the aeration of the suspension with air before the flotation of Cu, the desired oxidation-reduction potential of 60 to 340 mV is adjusted during the flotation of Cu by the aeration with air, the flotation of Cu is effected at a pH of 8.5 to 10.5 and Cu is removed from the flotation process with the froth.
机译:在用于选择性浮选铜铅锌硫化矿石的方法中,将原始矿石研磨并用水制成浆液,然后将所得悬浮液用空气充气以调节一定的氧化还原电位,然后依次用SO进行处理。 2,Ca(OH)2和收集和起泡剂,然后进行铜的浮选。通过在浮选铜之前用空气对悬浮液进行曝气,可以调节浮选所需的铜的氧化还原电位的70%至90%的氧化还原电位,所需的氧化还原电位为60至340 mV在用空气充气浮选铜的过程中,调节pH值,在pH为8.5-10.5的条件下进行浮选,并用泡沫从浮选过程中除去铜。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号