FIELD: metallurgy. SUBSTANCE: concentrate is fed by two stages: at the first stage 70-78% concentrate of its consumption per a melt in the mixture with flux is fed following by pouring after working of slag formed with silicomanganese. At the second stage residual part of concentrate after chemical enriching in the mixture with flux is fed. After attainment of required silicon concentration metal together with slag is put out. Ratio of concentrate after chemical enriching and fresh-fired flux is maintained at the first and second stages ( 2,25-2,55): and (1,6-1,8): 1, respectively. At the second stage 1-2% pieced limestone or dolomite is added to the mixture concentrate/flux. All mixture is attached by portions. EFFECT: improved method of smelting. 3 cl, 2 tbl
机译:领域:冶金。物质:精矿分两个阶段进料:在第一阶段,在与硅锰形成的炉渣进行加工后进行浇筑,然后将其与熔剂的混合物中每熔体消耗的70-8%的精矿进料。在第二阶段,将经过化学富集的具有助熔剂的混合物中的精矿剩余部分进料。在达到所需的硅浓度后,将金属与炉渣一起倒出。化学浓缩后和新烧助焊剂后精矿的比例分别保持在第一阶段和第二阶段(2,25-2,55):和(1,6-1,8):1。在第二阶段,将1-2%的石灰石或白云石粉加入到浓缩液/熔剂混合物中。所有混合物均分批连接。效果:改进的冶炼方法。 3厘升,2汤匙

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号