The limonite or mixtures of limonite / saprolite containing nickel are reduced to a heat in the form of pellets with a solid reducing agent and at a concentration of carbon dioxide. & br / the pellets are introduced into a reactor and heated gradually, with a reduction of the constituents metalliferous. They are then maintained at a temperature sufficiently high to allow the migration in the liquid phase of the substances to the inside of the pellets, but less than the point where the pellets become sticky. The atmosphere of this "zone of growth is checked with care in order to prevent the continuation of the reduction or a reoxidation, which provides a good environment for the growth of metal particles. The pellets are then cooled rapidly in order to avoid the conversion of wustite of magnetite and ground and the magnetic fraction is separated. & br / applicable to the extraction of nickel of minerals low.
机译:含镍的褐铁矿或褐铁矿/腐泥土的混合物以固体还原剂的形式和在二氧化碳浓度下以小球形式还原成热。 &将粒料引入反应器中并逐渐加热,同时减少了含金属的成分。然后将它们保持在足够高的温度下,以允许物质在液相中迁移到丸粒内部,但小于丸粒变粘的点。仔细检查“生长区”的气氛,以防止还原或再氧化的继续,这为金属颗粒的生长提供了良好的环境。然后将球团快速冷却,以避免金属颗粒的转化。磁铁矿与地面的铁橄榄石和磁性部分分离。适用于低矿物含量的镍的提取。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号