摘要

A vibration damping alloy has a mixed structure of martensite and austenite. The alloy steel is iron-based to which 14-22% by weight of manganese is added. The vibration damping alloy is manufactured by mixing electrolytic iron and manganese in a molten state. The molten mixture, containing 14-22% of manganese with the remainder of iron, is cast as an ingot. The ingot is homogenized at 1000°-1300° C. for 20-40 hours and then hot rolled at 900°-1100° C. for 20 minutes to 90 minutes. The ingot is cooled with air or water.
机译:减振合金具有马氏体和奥氏体的混合结构。合金钢是铁基的,其中添加了14-22重量%的锰。减振合金是通过将电解铁和锰以熔融状态混合而制造的。含有14-22%的锰和其余铁的熔融混合物被铸成铸锭。将铸锭在1000°-1300°C下均质20-40小时,然后在900°-1100°C下热轧20分钟至90分钟。锭用空气或水冷却。