PURPOSE:To stably maintain molten metal surface level in a pouring hole and further, to enable control under few frequency of opening/closing a valve for air supply as less as possible by parallel arranging a leakage compensating piping providing an electrically operated type flow rate control valve to an air supply control piping. CONSTITUTION:At first, in order to start the pouring, by closing a solenoid valve 21 in exhaust control piping 14, and opening a solenoid valve 16 in the air supply control piping 12, a solenoid valve 18 in the leakage compensating piping 13 and the electrically operated type flow rate control valve 19, pressure in a pressurizing chamber 4 is raised and the molten metal surfaces in the pouring hole 2 and molten metal receiving hole 3 are raised, and at the time of being brought into contact with a detecting element 6 of molten metal surface level for controlling air supply, the signal is received to close the solenoid valve 16 in the air supply control piping 12. Successively, by opening/closing a stopper 8 in a constant quantitative shotting device 10, the molten metal is poured in each one shot. By this method, to the leakage quantity changing in accordance with variation of the molten metal surface level in the pressurizing chamber 4 during shotting, as the leakage compensating control is executed by intermittently operating an electric motor in the electrically operated type flow rate control valve 19 to adjust the opening/closing velocity of the valve, the molten metal surface level in the pouring hole 2 is maintained to almost constant and the opening/ closing motion in the solenoid valve 16 can be executed at the necessary min. limit of the frequency.
机译:用途:为了稳定地保持浇铸孔中的熔融金属表面水平,并通过平行布置一个提供电动式流量控制的泄漏补偿管路,在开闭气源的频率尽可能少的情况下进行控制供气控制管路上的阀门。组成:首先,为了开始浇注,请关闭排气控制管路14中的电磁阀21,并打开空气供应控制管路12中的电磁阀16,泄漏补偿管路13中的电磁阀18和在电动式流量控制阀19中,加压室4内的压力上升,注入孔2和熔融金属接收孔3内的熔融金属表面升高,并且在与检测元件6接触时。在用于控制空气供应的熔融金属表面高度的变化过程中,接收信号以关闭空气供应控制管道12中的电磁阀16。接着,通过在恒定定量喷射装置10中打开/关闭塞子8,将熔融金属倒入在每一个镜头。通过该方法,由于在喷射期间根据加压室4中的熔融金属表面液位的变化而导致的泄漏量的变化,通过在电动式流量控制阀19中间歇地使电动机运转来进行泄漏补偿控制。为了调节阀的开/关速度,浇注孔2中的熔融金属表面水平保持几乎恒定,并且电磁阀16中的开/关运动可以在必要的最小时间执行。频率限制。

著录项

  • 公开/公告号JPH0787983B2

    专利类型

  • 公开/公告日1995-09-27

    原文格式PDF

  • 申请/专利权人 株式会社広築;

    申请/专利号JP19880259847

  • 发明设计人 南 省三;中安 斌;

    申请日1988-10-14

  • 分类号B22D39/06;

  • 国家 JP

  • 入库时间 2022-08-22 04:27:47

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号