首页> 外国专利> PRODUCTION OF HIGH-STRENGTH AUSTENITIC-FERRITIC STAINLESS STEEL

PRODUCTION OF HIGH-STRENGTH AUSTENITIC-FERRITIC STAINLESS STEEL

机译:高强度奥氏体-铁素体不锈钢的生产

摘要

PURPOSE: To form the structure of high-strength austenitic-ferritic stainless steel into an ultrafine-grained one and to improve its mechanical properties without deteriorating its ductility. ;CONSTITUTION: This high-strength austenitic-ferritic stainless steel having an ultrafine-grained structure is produced so that the powder of austenitic-ferritic stainless steel with 40 to 100μm powder size of austenite-ferrite two phases or a ferrite single phase of supersaturated solid solution is subjected to intense working by a mechanical alloying method, then rapidly heated from a room temp. to a solidifying temp. of 1000 to 1020°C, succeedingly subjected to compacting by executing hot rolling at 40 to 70% draft or hot extrusion at 5 to 15 extrusion ratio, and immediately subjected to rapid cooling to a room temp. In this producing method, heating from a room temp. to a solidifying temp. of 1000 to 1020°C can be regulated to ≤15min at the latest.;COPYRIGHT: (C)1995,JPO
机译:用途:将高强度奥氏体-铁素体不锈钢的组织形成超细晶粒,并在不降低其延展性的情况下提高其机械性能。 ;组成:生产具有超细晶粒结构的高强度奥氏体-铁素体不锈钢,以使奥氏体-铁素体不锈钢的粉末具有40至100μm的奥氏体-铁素体两相或铁素体单相的粉末尺寸溶液通过机械合金化方法进行剧烈加工,然后从室温快速加热。到凝固的温度在1000至1020℃的温度下,通过以40至70%的牵伸率进行热轧或以5至15的挤压比进行热挤压而随后进行压实,并立即进行快速冷却至室温。在该制造方法中,从室温开始加热。到凝固的温度最高可调节至1000至1020°C≤15分钟。;版权所有:(C)1995,日本特许厅

著录项

  • 公开/公告号JPH0734181A

    专利类型

  • 公开/公告日1995-02-03

    原文格式PDF

  • 申请/专利权人 KOBE STEEL LTD;

    申请/专利号JP19930195392

  • 发明设计人 NAGAO MAMORU;MIYAMOTO ATSUYUKI;

    申请日1993-07-13

  • 分类号C22C33/02;C21D8/00;

  • 国家 JP

  • 入库时间 2022-08-22 04:22:09