Silver alloy for craftwork -- obtd., by the photography from other metals and other wastes and contg.Small amts.Silver recycling

机译:用于手工制作的银合金-由摄影,其他金属和其他废料制成,并包括小规模的银回收

摘要

PCT numbers PCT/DE94/00007 seconds. 371 conclude the age of second on the 24th July in 1995. 102 August 4th PCT publication numbers on January 7 WO94/17004 PCT publication dates of 1995 (e) date PCT 1994 on July 24 submit, the method that 1994In is used to generate the insulating materials of the bound control with environmental protection, one long chained starch is used as adhesive, in addition to silicone. Starch is heated up to 50 degree to 60 degrees Celsius, keeps in this temperature and respectively sprays on the glass fibers from silicone; It is made of using 6 to 8% adhesive starch and silicone, then one pulls into Filamentous glass mat or slab and can be shaped and dry at about 180 degrees Celsius. One to pull into Filamentous glass mat (16), insulated target or slab or absorber be that thus obtained its surprisingly waterproof and is uniquely combined, resin and silicone by starch, can unquestionably using and always with a uniform bulk density. It is providing in that purpose plant (1), providing for water (9), for starch (10) and for the supply ring of silicone (11). Nozzle (13) for supply ring 10 has large opening and separation edge. Premixing container (17) and feed pipe (15) are heatable or heat-insulated. In another embodiment, a latex is made of silicone resin, silicone oil, a dust binder and starch, is atomized and is sprayed to 200 degrees Celsius at 18 degree on the stream of the process of glass fibre.
机译:PCT编号PCT / DE94 / 00007秒。 371表示1995年7月24日为第二年龄。102 8月4日PCT公开号为1月7日,WO94 / 17004 PCT公开日期为1995年(e),PCT 1994年为7月24日,提交时使用了1994In方法环保控制的绝缘材料,除了硅酮外,还使用一种长链淀粉作为粘合剂。淀粉加热到50摄氏度至60摄氏度,保持在此温度下,并分别从硅树脂喷洒到玻璃纤维上;它是由6%至8%的粘性淀粉和硅酮制成,然后将其拉入丝状玻璃毡或平板中,并可以在约180摄氏度的温度下成型和干燥。如此插入到丝状玻璃垫(16),绝缘的靶材或平板或吸收器中的方法是,其具有令人惊讶的防水性,并且独特地结合了淀粉和树脂和有机硅,可以毫无疑问地使用并且始终具有均匀的堆积密度。在该目的中,其提供设备(1),水(9),淀粉(10)和硅酮(11)的供应环。供给环10的喷嘴(13)具有较大的开口和分离边缘。预混合容器(17)和进料管(15)是可加热的或隔热的。在另一个实施方案中,将由硅树脂,硅油,粉尘粘合剂和淀粉制成的胶乳雾化,并在玻璃纤维工艺流中以18摄氏度的温度喷涂至200摄氏度。

著录项

  • 公开/公告号NO952751L

    专利类型

  • 公开/公告日1995-07-11

    原文格式PDF

  • 申请/专利权人 SCHIWEK HELMUT;

    申请/专利号NO19950002751

  • 发明设计人 SCHIWEK HELMUT;

    申请日1995-07-11

  • 分类号C03C25/02;

  • 国家 NO

  • 入库时间 2022-08-22 04:18:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号