首页> 外国专利> Re-calcination and extraction process for the detoxification and comprehensive utilization of chromic residues

Re-calcination and extraction process for the detoxification and comprehensive utilization of chromic residues

机译:重新煅烧和提取工艺用于铬渣的解毒和综合利用

摘要

A re-calcination and extraction process for the detoxification and comprehensive utilization of chromic residues, comprising adding small amount of residue ore powder, sodium carbonate, or additionally, a certain amount of coke powder to the poisonous chromic residues, and calcining the mixture in a re-calcinating apparatus at 1000-1200. degree. C., for 30-60 minutes. The re-calcined grog is extracted with water, to obtain an extractive liquor containing sodium chromate. The extractive liquor can be used to produce chromium oxide, basic chromium sulfate or medium chrome yellow; while the extracted residues can be sintered at high temperatures with iron ore powder and coke to obtain a massive self-melting sintered iron, which can be further converted to a low-chromium cast iron. This process can thoroughly detoxify the chromic residues, effectively recover Cr2O3 and remove water-soluble Cr+6, whereby various important industrial materials are produced. The method brings very good economical and environmental benefits.
机译:一种用于铬渣的脱毒和综合利用的重煅烧和萃取工艺,包括向有毒的铬渣中添加少量的渣粉,碳酸钠或另外的一定量的焦粉,然后在有毒的铬渣中煅烧混合物。重新煅烧设备在1000-1200。度。 C. 30-60分钟。用水萃取重新煅烧的熟料,以获得含有铬酸钠的萃取液。萃取液可用于生产氧化铬,碱性硫酸铬或中等铬黄;提取的残渣可以在高温下与铁矿粉和焦炭一起烧结,以获得块状的自熔烧结铁,然后可以进一步转化为低铬铸铁。该方法可以彻底去除铬残留物的毒性,有效回收Cr2O3并去除水溶性Cr + 6,从而生产出各种重要的工业材料。该方法带来了很好的经济和环境效益。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号