首页> 外国专利> AUSTENITIC STAINLESS STEEL FOR HIGH SPEED CONTINUOUS PRESS WORKING EXCELLENT IN SEASON CRACKING RESISTANCE

AUSTENITIC STAINLESS STEEL FOR HIGH SPEED CONTINUOUS PRESS WORKING EXCELLENT IN SEASON CRACKING RESISTANCE

机译:奥氏体不锈钢,具有出色的抗开裂性能,可用于高速连续冲压加工

摘要

PURPOSE: To prevent the generation of cracks in a stainless steel in the case of high speed continuous press working by incorporating specified amounts of C, Si, Mn, Ni, Cr, Cu, N Mo and Fe therein. ;CONSTITUTION: The compsn. of this stainless steel is constituted of the one contg., by weight, ≤0.05% C, 1 to 2.5% Si, ≤5% Mn, 5 to 9% Ni, 14 to 19% Cr, ≤4% Cu, 0.04% Ni and ≤1% Mo, and the balance substantial Fe. Moreover, (C+N); 0.06 and (a) value; -0.3 to 1 are satisfied; where (a) value = 19.43-10.8 C-0.14Si-0.54Mn-1.02Ni-0.57Cr-0.49Cu-7.53N. As for the relationship between the ratio of the amt. of a martensitic phase to the amt. of an austenitic phase and the amt. of work strain, the (a) value is introduced from the experimental result. In the case the (a) value is small, the austenitic phase can be valued as being stable. Multistage press working can be executed by high speed continuous pressing.;COPYRIGHT: (C)1996,JPO
机译:目的:为防止在高速连续冲压加工过程中不锈钢中产生裂纹,可在其中加入指定量的C,Si,Mn,Ni,Cr,Cu,N Mo和Fe。 ;组成:compsn。该不锈钢的重量百分比为:≤0.05%C,1-2.5%Si,≤5%Mn,5-9%Ni,14-19%Cr,≤4%Cu,0.04% Ni和Mo≤1%,其余部分为Fe。此外,(C + N); <0.06和(a)值; -0.3至1满足; (a)值= 19.43-10.8 C-0.14Si-0.54Mn-1.02Ni-0.57Cr-0.49Cu-7.53N。至于amt的比例关系。到amt的马氏体相。奥氏体相和amt。对于工作应变,从实验结果中引入(a)值。在(a)值小的情况下,奥氏体相可以被认为是稳定的。可以通过高速连续压制进行多级压制工作。版权所有:(C)1996,日本特许厅

著录项

  • 公开/公告号JPH08269638A

    专利类型

  • 公开/公告日1996-10-15

    原文格式PDF

  • 申请/专利权人 NISSHIN STEEL CO LTD;

    申请/专利号JP19950092017

  • 申请日1995-03-27

  • 分类号C22C38/00;C22C38/40;C22C38/58;

  • 国家 JP

  • 入库时间 2022-08-22 04:03:44

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号