Recovery of alkali and alkaline earth chlorides (I) from waste salts from heat treatment of steel pts. in salt baths involves dissolving the waste salt components in water, sepg. the insol. residue, destroying cyanides if necessary and fractional crystallisation of the dissolved salts. BaCO3 is sepd. from the residue as BaCl2 by adding HCl and added to the salt soln.. BaCl2 is crystallised from the salt soln. by adding NaCl and CaCl2 in (1-5):1 ratio at -5 to +20 degrees C using 150-350g NaCl and 30-150g CaCl2 to 300 g/l waste salt in soln.. NaCl is crystallised by adding CaCl2 to a concn. of 150-400 g/l at 40-120 degrees C. Residual NaCl and BaCl2 are crystallised by concentrating the soln. by evapn. to a CaCl2 concn. of 5500-900 g/l at 60-120 degrees C. A KCl-CaCl2 double salt is crystallised by further concn. at 60-120 degrees C, then the double salt is dissolved in 20-35% CaCl2 soln. at 35-40 degrees C and KCl is crystallised at 5-20 degrees C. CaCl2 is recovered by evaporating the remaining soln. to dryness.
机译:从钢pts的热处理废盐中回收碱金属和碱土金属氯化物(I)。在盐浴中,包括将废盐成分溶解在水中。日晒。残留物,必要时破坏氰化物,并使溶解的盐分步结晶。 BaCO3为Sepd。通过加入HCl从残余物中以BaCl 2的形式从残余物中分离出BaCl 2。从盐溶液中结晶出BaCl 2。通过在150至350 g / l废盐溶液中在150至350 g的NaCl和30至150 g的CaCl 2在-5至+20摄氏度下以(1-5):1的比例添加NaCl和CaCl 2来实现。一个concn。在40-120℃下,其熔点为150-400g / l。通过浓缩溶液使残留的NaCl和BaCl 2结晶。通过evapn。到氯化钙溶液中在60-120℃下将其溶于5500-900g /l。KCl-CaCl2复盐通过进一步浓缩而结晶。在60-120摄氏度下,将复盐溶于20-35%的CaCl2溶液中。在35-40℃下蒸发KCl,在5-20℃下结晶。通过蒸发残留的Soln回收CaCl2。干燥。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号