摘要

(1);(R 1-x L x ) (Ni ly M y ) z (1);Mg, Ca, M, Co, Al, Mn, Fe, Cu, Zr (R, La, Ce, Pr, Nd, L: Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Y, Sc, , Ti, Mo, Si, V, Cr, Nb, Hf, Ta, W, B, C, 0.05? X? 0.4, 0? Y? 0.5, 3.0? Z 4.5) Wherein an opposite phase boundary perpendicular to the C axis of the crystal grains contains not less than 5 and not more than 25 but less than 95 and less than 95% Wherein at least 60% and less than 95% of the elements are placed in the reverse phase region, and a method for producing the rare earth metal-nickel-based hydrogen storage alloy.
机译:(1);(R 1-x L x )(Ni ly M y z (1); Mg,Ca,M,Co,Al,Mn,Fe,Cu,Zr(R,La,Ce,Pr,Nd,L:Gd,Tb,Dy,Ho,Er,Tm, Yb,Lu,Y,Sc ,,, Ti,Mo,Si,V,Cr,Nb,Hf,Ta,W,B,C,0.05≤X≤0.4,0≤Y≤0.5,3.0≤Z <4.5)垂直于晶粒的C轴的相反相界包含不少于5且不超过25但少于95且少于95%,其中至少60%且少于95%的元素反过来放置相区域和用于制备稀土金属-镍基储氢合金的方法。

著录项

  • 公开/公告号KR970705652A

    专利类型

  • 公开/公告日1997-10-09

    原文格式PDF

  • 申请/专利权人 이노우에 유스케;

    申请/专利号KR19970701526

  • 发明设计人 가네코 아키히토;

    申请日1997-03-08

  • 分类号C22C19/00;H01M4/38;

  • 国家 KR

  • 入库时间 2022-08-22 03:16:07