首页> 外国专利> Glass-ceramic sintered body, a process for its preparation and a glass- ceramic substrate

Glass-ceramic sintered body, a process for its preparation and a glass- ceramic substrate

机译:微晶玻璃烧结体,其制备方法和微晶玻璃基板

摘要

A glass-ceramic sintered body comprising an SiO.sub.2 --Al.sub. 2 O.sub. 3 --MgO--ZnO--B.sub.2 O.sub.3 type crystalline glass and alumina, said sintered body containing at least 10% by weight of a spinel crystalline phase; and a substrate composed of the sintered material. There is also provided a process for producing the glass-ceramic sintered body which comprises adding a binder to a mixed powder of an SiO.sub.2 -- Al.sub.2 O. sub.3 --MgO--ZnO--B.sub.2 O.sub.3 type crystalline glass and alumina, molding the mixture into a predetermined shape, and firing the mixture into a predetermined shape, and firing the molded mixture at a temperature of 925° to 1000° C. in a non-oxidizable atmosphere. The glass-ceramic sintered body and the substrate composed of it in accordance with the present invention have excellent mechanical strength and thereby have markedly increased metallizing adhesion strength.
机译:包含SiO 2 -Al的玻璃陶瓷烧结体。 2 O.sub。 3 -MgO-ZnO-B 2 O 3型晶体玻璃和氧化铝,所述烧结体包含至少10重量%的尖晶石晶体相;由烧结材料构成的基板。还提供了一种用于制造玻璃陶瓷烧结体的方法,该方法包括将粘合剂添加到SiO 2 -Al 2 O 3 -MgO-ZnO-的混合粉末中。 B 2 O 3型结晶玻璃和氧化铝,将混合物模制成预定形状,并将混合物烧成预定形状,然后在925℃至1000℃的温度下烧成模制混合物。不可氧化的气氛。根据本发明的玻璃陶瓷烧结体和由其构成的基材具有优异的机械强度,从而具有显着提高的金属化粘合强度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号