首页> 外国专利> BERYLLIUM-NICKEL-COPPER LEAN ALLOY HAVING HIGH ELECTRIC CONDUCTIVITY AND STRESS RELAXATION RESISTANCE

BERYLLIUM-NICKEL-COPPER LEAN ALLOY HAVING HIGH ELECTRIC CONDUCTIVITY AND STRESS RELAXATION RESISTANCE

机译:具有高电导率和抗应力松弛性能的铍镍铜纯铜合金

摘要

PROBLEM TO BE SOLVED: To provide a beryllium-nickel-copper lean alloy having high electric conductivity and stress relaxation resistance. ;SOLUTION: This alloy has a composition represented by a composition formula which consists of 0.15-0.5& Be, 0.40-1.25& Ni, 0-0.25& Sn, 0.06-1% Zr and/or 0.06-1% Ti, and the balance copper and in which the total content of Zr and Ti is regulated to about 0.06-1%0 In this alloy, electric conductivity, bendability, and stress relaxation resistance are improved without deteriorating strength.;COPYRIGHT: (C)1998,JPO
机译:要解决的问题:提供一种具有高电导率和抗应力松弛性能的铍-镍-铜贫合金。 ;解决方案:该合金的组成由以下组成公式表示:0.15-0.5&Be,0.40-1.25&Ni,0-0.25&Sn,0.06-1%Zr和/或0.06-1%Ti和平衡的铜,其中Zr和Ti的总含量控制在0.06-1%0左右。在这种合金中,导电性,弯曲性和抗应力松弛性得到改善,而不会降低强度。;版权所有:(C)1998,JPO

著录项

  • 公开/公告号JPH10183276A

    专利类型

  • 公开/公告日1998-07-14

    原文格式PDF

  • 申请/专利权人 BRUSH WELLMAN INC;

    申请/专利号JP19970295671

  • 发明设计人 WOLF SHELLEY J;HARKNESS JOHN C;

    申请日1997-10-28

  • 分类号C22C9/06;C22F1/08;

  • 国家 JP

  • 入库时间 2022-08-22 03:07:57

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号