Ensure chromium steel made of the method for optimal creep resistant product quality

机译:确保采用该方法制成的铬钢具有最佳的抗蠕变产品质量

摘要

Method ensures the chemical composition of optimal flame retardant property chromium steel product, and quality percentage indicates there is value: 0.05 to 0.25% carbon in this regard; 0.01 to 0.5% manganese; 0.01 to 0.5% silicon; 8 to 14% chromium, 0.2 to 1.8% molybdenum; Up to 2.2% micro tungsten, 0.05 to 0.3% vanadium; 0.02 to 0.2% niobium; 0.03 to 0.1% nitrogen; Up to 1.5% micro nickel; The copper of up to 2.0% up to 3% micro and trace, cobalt, slag iron attach element and common impurities. The product is heated to 1180 to 1220 degrees Celsius and subsequent cooling in empty gas and water and oil and 100 to 20 degrees Celsius. Then,Heat product to 1030 to 1070 degrees Celsius and cool sky gas and water or oil, be cooled to 100 to 20 degrees Celsius and subsequent tempering at 600 to 780 degrees Celsius around temperature.IMAGE
机译:该方法确保了最佳阻燃性能的铬钢产品的化学成分,并且质量百分比表明有该值:在这方面碳为0.05至0.25%; 0.01至0.5%锰; 0.01至0.5%的硅;铬8至14%,钼0.2至1.8%;最高2.2%的微量钨,0.05至0.3%的钒; 0.02至0.2%铌; 0.03至0.1%氮;镍含量高达1.5%;高达2.0%的铜和高达3%的微量和痕量的钴,炉渣铁附着元素和常见杂质。将产品加热到1180至1220摄氏度,然后在空的气体,水和油中以及100至20摄氏度下冷却。然后,将产品加热到1030至1070摄氏度,并冷却天空燃气和水或油,冷却至100至20摄氏度,然后在温度范围内以600至780摄氏度回火。

著录项

  • 公开/公告号CZ124496A3

    专利类型

  • 公开/公告日1998-03-18

    原文格式PDF

  • 申请/专利权人 VITKOVICE;

    申请/专利号CZ19960001244

  • 申请日1996-04-30

  • 分类号C21D1/78;C21D1/18;

  • 国家 CZ

  • 入库时间 2022-08-22 02:58:30

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号