Sol-Gel Method of obtaining pure or mixed zirconium oxide balls, microspheres and transfer, usable as catalyst or catalyst carrier

机译:Sol-Gel获得纯或混合的氧化锆球,微球和转移的方法,可用作催化剂或催化剂载体

摘要

Process for obtaining pure or mixed oxide zirconia spheres, microspheres or washcoats consisting of: preparing a zirconium solution in water at a concentration, formally expressed as ZrO2, equal or lower than 400 g/l, starting from a basic zirconium carbonate additioned of conc. nitric acid up to a molar ratio ÄNO3-Ü/ÄZr4+Ü between 0.8 and 1.1, and eventually preparing one or more solutions of the other oxides when necessary; preparing a sol of zirconium, eventually mixed to other metals, by a thickening agent and, in the case of spheres and microspheres, of a surface active agent too; dripping the sol into an alkaline gelation bath for obtaining gel spheres or microspheres, or sucking the sol into the honeycomb channels in order to obtain the washcoats, with subsequent gelation with gaseous ammonia; ageing the so obtained gel; rinsing with water down to pH = 9-10, only in the case of gel spheres or microspheres; drying and calcining. IMAGE
机译:获得纯的或混合的氧化锆球,微球或修补基面涂层的方法,该方法包括:从水中加入浓度为400克/升的正式表示为ZrO2的锆溶液,以正式表示为ZrO2的浓度制备。硝酸,直至ÄNO3-Ü/ÄZr4++Ü的摩尔比在0.8和1.1之间,并在必要时最终制备一种或多种其他氧化物的溶液;制备锆溶胶,并最终通过增稠剂以及在球形和微球的情况下还通过表面活性剂与其他金属混合;将溶胶滴入碱性凝胶浴中以获得凝胶球或微球,或将溶胶抽吸至蜂窝通道中以获得载体涂层,随后与气态氨进行凝胶化;使如此获得的凝胶老化;仅在凝胶球或微球的情况下,用低至pH = 9-10的水冲洗;干燥和煅烧。 <图像>

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号